Old 03-15-2008, 01:37 AM   #1

bblauvelt is currently offline
Posts: 20
Status: First Lieutenant
Join Date: Jan 2008
Gallery Images: 0


Thanks: 0
Thanked 0 Times in 0 Posts
Send bblauvelt:
a Private Message
 
Default Bravo III + Stainless Skeg Guard = Galvanic corrosion (Yes/No?)

I have very minor damage to my Skeg which I bought a Skeg Gauard to cover so I don’t need to be reminded what the trailer switch in a Z272 does. However, now I’m thinking I shouldn't use it because it may increase the Galvanic corrosion.

Question 1: Should I bother with Skeg Guard or will it increase the galvanic corrosion?

Question 2: Does anyone know if the mercathode still receives power when the battery switch is off or how I can test it has power?


Here’s my water and anode configuration:

I keep the boat in a slip were the river changes from brackish to fresh. When I bought the boat I read up on the Bravo III and found they are prone to galvanic corrosion problems. Because of this I decided to add a prop anode since my Bravo III is pre-2003. I have Stainless props and used magnesium anodes last season. My anodes were consumed around 50-60% between May-October. I painted the unit myself last season but this year it was refinished since I had the boat in the shop getting other work.
Reply With Quote
  • Old 03-15-2008, 08:19 AM   #2
     
    WetWilly's Avatar

    WetWilly is currently offline
    Posts: 2,205
    Status: INACTIVE
    Join Date: Sep 2007
    Location: SF Bay Area, Ca.
    Find me on the Map
    My Year: 1996
    My Model: Z240 Talari
    My Engine: 7.4L Bravo III
    Gallery Images: 25


    Thanks: 3
    Thanked 110 Times in 55 Posts
    Send WetWilly:
    a Private Message
     
    Default

    Hello bblauvelt,

    Question 1: Should I bother with Skeg Guard or will it increase the galvanic corrosion?

    Since it is a different metal than the outdrive, yes, but the real question is how much and that is difficult to tell. Now do you need it, No, not really unless you are prone to damaging the skeg because of the area where you boat or the occasional moment of memory loss when hauling your boat onto a trailer.


    Question 2: Does anyone know if the Mercathode still receives power when the battery switch is off or how I can test it has power?

    If wired up properly, Yes, it should have power all the time to provide constant protection (click here to see the different Mercathode systems and how they're wired).

    You can test to see if it’s getting power but to determine if it is working properly requires proper testing
    (click here). Your Authorized Mercruiser Service Center can check your system for proper operation and since yours sits in brackish water a lot, I suggest a regular check of the system for peace of mind. I just had mine repaired, the controller went bad.


    Do you have the anode above the cavitation plate in the front of the lower outdrive? If not, see about having it installed. I'm glad to hear you're using the magnesium anodes instead of the aluminum, it makes a big difference.



    WetWilly

    Last edited by WetWilly; 03-15-2008 at 08:22 AM.
    Reply With Quote
    Old 03-18-2008, 01:27 AM   #3

    bblauvelt is currently offline
    Posts: 20
    Status: First Lieutenant
    Join Date: Jan 2008
    Gallery Images: 0


    Thanks: 0
    Thanked 0 Times in 0 Posts
    Send bblauvelt:
    a Private Message
     
    Default

    Thanks for the information. I've decided not to put on the SkegGuard. My primary fear is the mounting holes. It just seems to reason there is no way to protect the inside surface of the hole drilled in the Skeg. I really don't want to find out that the 1/4 holes become 1/2 down the road. The chip the Skeg only bothers me when it's on the trailer and I can't see it once I'm back in the slip.
    Reply With Quote
    Old 03-19-2008, 01:37 AM   #4
     
    jmills224's Avatar

    jmills224 is currently offline
    Posts: 55
    Status: First Mate
    Join Date: Jul 2007
    Location: Oklahoma
    Find me on the Map
    My Model: 1997 179SE Talari 4.3LX Gen+/Alpha1 Gen II
    Gallery Images: 4


    Thanks: 0
    Thanked 0 Times in 0 Posts
    Send jmills224:
    a Private Message
     
    Default

    I saw this the other day on Overtons web page. Its a skeg protector thats made of nylon comosite.

    http://www.overtons.com/modperl/prod...ID=1008&r=view

    I'm thinking of getting one for my boat.
    Reply With Quote
    Old 03-19-2008, 03:50 AM   #5
     
    WetWilly's Avatar

    WetWilly is currently offline
    Posts: 2,205
    Status: INACTIVE
    Join Date: Sep 2007
    Location: SF Bay Area, Ca.
    Find me on the Map
    My Year: 1996
    My Model: Z240 Talari
    My Engine: 7.4L Bravo III
    Gallery Images: 25


    Thanks: 3
    Thanked 110 Times in 55 Posts
    Send WetWilly:
    a Private Message
     
    Default

    Thanks jmills224,

    Looks like you found a real viable alternative to the SS Skeg Guards!

    Here's their site: Blackfin Skeg

    Did a little Google and found some interesting reviews...
    Review #1 and Review #2

    Now I'm contemplating going with the Blackfin and from what I'm reading, the real issue is getting it to stay on and I believe it's all in the prep and gluing that makes the difference.

    Check out this
    clip where they beat up on the Blackfin and it seems to holds up great in the video.

    Think I'll call Blackfin tomorrow for a little more info.

    WetWilly
    Reply With Quote
    Old 03-19-2008, 02:25 PM   #6
     
    indykoch's Avatar

    indykoch is currently offline
    Posts: 622
    Status: Platinum Contributor
    Join Date: Jul 2007
    Location: Fishers, IN
    Find me on the Map
    My Year: 1999
    My Model: Z212 Shabah
    My Engine: 350 Magnum Alpha One
    Gallery Images: 18


    Thanks: 0
    Thanked 26 Times in 24 Posts
    Send indykoch:
    a Private Message
     
    Default

    I don't know Willy... That video, while amusing, didn't impress me much. The guy didn't look like he was really swinging that hard, the lower unit wasn't even attached to anything allowing it to absorb some of the shock, and the truck running over it is like driving over a flat piece of plastic with soft tires - what could break???

    And anyone that uses "dagum" in his advertisement makes me reconsider the validity of the message.

    He sure makes an awful lot of promises too. Something that will get him in trouble.

    I don't need the skeg guard yet, but I think I'm a fan of the stainless version.
    __________________
    Ryan
    Previously - '99 Z212 Shabah
    350 Mag MPI
    Currently - '07 Ebbtide 2600 CBR
    Reply With Quote
    Old 03-19-2008, 03:11 PM   #7

    mikeyt is currently offline
    Posts: 7,483
    Status: Platinum Contributor
    Join Date: Jul 2007
    Location: Ontario
    Find me on the Map
    My Year: 1996
    My Model: Shabah 180
    My Engine: 4.3
    Gallery Images: 14


    Thanks: 87
    Thanked 579 Times in 538 Posts
    Send mikeyt:
    a Private Message
     
    Default

    I think that it looks like a bit of a 'cheap' solution. There weren't that many positive opinions in the "Review #1" that Willy noted and i have trouble believing some of the reviews in the ones at retailers websites. I could use to put a skeg-guard on mine as i have a smallish chunk missing out of the rear of the skeg. The composite one seems a little 'bulkish' & i suspect it might cause a little extra drag at higher speeds. The SS one seems to have a much cleaner look and likely fits better but it comes at an additional $30-40.
    __________________
    Rarely visit this site given its problems and lack of management interest.
    Reply With Quote
    Old 03-19-2008, 08:29 PM   #8
     
    WetWilly's Avatar

    WetWilly is currently offline
    Posts: 2,205
    Status: INACTIVE
    Join Date: Sep 2007
    Location: SF Bay Area, Ca.
    Find me on the Map
    My Year: 1996
    My Model: Z240 Talari
    My Engine: 7.4L Bravo III
    Gallery Images: 25


    Thanks: 3
    Thanked 110 Times in 55 Posts
    Send WetWilly:
    a Private Message
     
    Default

    Hi indykoch and mikeyt,

    I agree with the both of you, as for the video, yea, it looks pretty hokey...and doesn't really prove anything as well. Now if they bolted it down, took a an oak 4x4 and gave it a Barry Bonds swing....

    From what I'm sensing, this works best on outboards, by design, they pop up much easier and faster after an underwater strike than an IO does so a good part of the the impact energy would be transfered into motion.

    I'm still willing to give it a go, you never know, it might just be as good as they say, than again.....

    I'll let you know when I have more info on it!

    WetWilly
    Reply With Quote
    Old 03-20-2008, 06:14 PM   #9
     
    MariahMan's Avatar

    MariahMan is currently offline
    Posts: 1,232
    Status: Admin Guy
    Join Date: Jun 2007
    Location: Seattle, WA
    Find me on the Map
    My Year: 2001
    My Model: 252 Shabah
    My Engine: Volvo Penta 5.7GXi, DP
    Gallery Images: 211


    Thanks: 10
    Thanked 204 Times in 36 Posts
    Send MariahMan:
    a Private Message
     
    Default

    Interesting....I didn't know skeg breakage was that common. On our Volvo outdrive, the skeg is THICK cast iron as the rest of the drive assembly is. Seems like it would be hard to break that and not break the trim cylinders themselves.

    From what i know, an impact like the ones showed in the video underwater underway would cause the trim cylinders to either break or release. I think some of them have a some sort of release that, upon sudden impact, allows the drive to kick up. It's far better to replace trim cylinders than repari the hull damage and replace the outdrive if it were to rip off the boat.

    The Blackfin guys' argument that with this device, your outdrive and prop will be protected from damage is pretty rediculous. No skeg attachment will protect your prop from damage. It doesn't take much to bend a prop going down the lake if you clip a branch or other debris in the water. I know from experience.
    __________________
    -Ryan

    ThunderShark Web Solutions
    PM or email me if you need hosting or community support.
    Reply With Quote
    Old 11-28-2009, 02:29 AM   #10

    backwater bill is currently offline
    Posts: 8
    Status: Stowaway
    Join Date: Nov 2009
    My Year: 2000
    My Model: Z222
    My Engine: 5.7 alpha one
    Gallery Images: 0


    Thanks: 0
    Thanked 0 Times in 0 Posts
    Send backwater bill:
    a Private Message
     
    Default Re: Bravo III + Stainless Skeg Guard = Galvanic corrosion (Yes/No?)

    I beg to differ Mariah Man. My Z222 hit some of the old bridge structure at Jone's pass and destroyed the bottom piece of the Blackfin but saved my props. Plus with the added surface area of the Blackfin my boat handles like a sports car. When i dock and trailer the boat responds much better with the "bigger rudder" without having to throttle up. If you see a skeg with all the paint then it hasn't been in the water yet.
    Reply With Quote
    Reply

    Bookmarks




    Currently Active Users Viewing This Thread: 1 (0 members and 1 guests)
     


    Similar Threads
    Thread Thread Starter Forum Replies Last Post
    Skeg & Stabilizer joez200 Original Mariah Talk 7 11-28-2009 01:32 PM
    Mariah Stainless Fuel Cover dieselwiezil Original Mariah Talk 8 07-15-2009 08:30 PM
    Wanted: Stainless Drink holders dudders Mariah Parts For Sale & Wanted 17 07-15-2009 01:33 AM
    Bravo III skeg repair finally finished WetWilly Original Mariah Talk 35 05-10-2009 08:29 AM
    Stainless Steal Carpet Snaps Douglas Alderman Chit Chat/Off-Topic 2 04-05-2008 04:53 AM



    Forum Right Top
    Forum Left Bottom Forum Right Bottom
     
    Right Left
    Member Login
    Forgot password?
    Forum LeftForum Right

    About the Club
    Age of the Mariah Owners Club:

    Total Members: 19,008
    Total Threads: 13,243
    Total Posts: 68,837
    Find us on Facebook Follow us on Twitter Subscribe to Mariah Owners Club on YouTube
    There are 288 users
    currently browsing forums.
    Forum LeftForum Right

    Find us on Facebook
    Forum LeftForum Right

    Club Sponsors
    Right Sponsor





    Forum LeftForum Right
    Right Right
    Right Bottom Left Right Bottom Right